ÖZKARDEŞLER · Label

Through-cutting or kiss-cutting in a label cutting die? Describe the liner correctly

Should the top surface of the label peel off smoothly while the bottom liner remains intact? The answer to this question determines the objective of the label cutting die. Saying "a label will be cut" is not enough to explain the difference between through-cutting and kiss-cutting.

The goal in kiss-cutting is to protect the liner

In a self-adhesive, liner-backed label, kiss-cutting aims to cut the layers that allow the label to separate from the liner while preserving the function of the liner. In through-cutting, the desired contour can be completely separated along with the liner. Therefore, state upfront whether the finished product will be used in sheets or individually.

This guide is for sheet-fed steel-rule cutting dies. The tooling geometry and setup of roll label systems are evaluated separately. Using the same concept does not mean different machine systems will use the same tooling.

Provide surface, adhesive, and liner information together

Coated or thermal paper, PP, or PET surfaces alone do not describe the entire label structure. The properties of the adhesive and liner, lamination, and other surface treatments are also included in the cutting evaluation. The supplier's product code and actual production sample make this information clearer.

Do not directly copy the previous setup when the material changes. Running the same design on a different liner does not automatically repeat the previous result.

Examine peeling and liner damage separately

Check whether the label peels cleanly on the test sheet, whether the contour is completed, and look for cutting or weakening marks on the liner separately. Compare different areas of the sheet instead of the result of a single up. Do not record recurring incomplete cuts in the same corner and randomly distributed defects with the same note.

Machine setup must be evaluated within the operator's authority and manufacturer instructions. Increasing pressure as soon as an incomplete cut is seen may mask liner damage or another tooling issue. First, record the current status and the location of the error.

Prepare the quote file with this distinction

  • Latest revised dimensioned contour and sheet layout.
  • Machine model, feed direction, and number of ups.
  • Material product code, surface, adhesive, and liner information.
  • Separate indication of lines requiring through-cutting/kiss-cutting.
  • Photo of the problematic sheet and related cutting die area, if any.

Contact Özkardeşler with the material sample and drawing information. Let us evaluate the cutting objective, machine compatibility, and required cutting die preparation in the same meeting.

Frequently asked questions

Is kiss-cutting the same process as creasing?

No. Kiss-cutting refers to the cutting depth objective in layered materials, whereas creasing refers to the process of forming a fold line.

Is the rule solely to blame if there is a mark on the liner?

This observation alone is not sufficient. The tooling, counter surface, pressure distribution, and material are examined together.

Coated stickers, thermal, PP, and PET labels are not the same structure

Opaque or transparent appearance does not define the face material, adhesive, and liner by itself. Share the layers and total thickness when requesting coated stickers, thermal paper, vellum, PP, PET, or PVC stickers. It should not be assumed that different application names like IML are inherently suitable for the same sheet steel-rule layout; the production method is examined separately.

8 mm and 12 mm label cutting rule: how should you specify the height?

Explore other cutting die technical guides

Technical preparation and application guides

Technical preparation and application guides