ÖZKARDEŞLER · TECHNICAL NOTES

Why doesn't the same grammage mean the same creasing adjustment?

Why are paperboard grammage and actual thickness evaluated together? A technical preparation guide for creasing-rule, channel, and material compatibility.

Writing the same grammage on a paperboard does not mean that two materials will fold in the same way. In die preparation, along with the grammage, it is necessary to know the actual thickness, material definition and the process to be applied.

Grammage and thickness are two different pieces of information

Grammage refers to the mass per unit area of the material; it is usually indicated in g/m². Thickness, on the other hand, is a separate property measured in mm or microns. Therefore, the grammage information should not be used directly as a thickness value.

For example, both paperboards can be 350 g/m². This information does not prove that both have the same thickness. In technical evaluation, requesting the exact product definition and measured thickness together reduces the risk of proceeding with assumptions.

Which measurements are evaluated together in creasing?

The creasing rule and counter channel are not selected independently of each other. The actual thickness of the paperboard, the characteristics of the creasing rule and the dimensions of the counter channel enter into the same evaluation. Manufacturer calculation aids can provide a starting point; the result given for a specific material and system should not be directly transferred to every application.

For this reason, we do not give a definitive channel or rule dimension with just the information "we use 350 gram paperboard". We prefer to clarify the material, machine and expected folding result together.

How should you handle the previous setting when the material changes?

The previous production record is a good reference. Assuming the new material is automatically equivalent to the previous one is a separate decision. If the supplier or paperboard series has changed, re-record the product definition, actual thickness, grain direction and any printing/coating processes. Make the result evaluation with the material to be used in production.

During inspection, it is not sufficient to look only at the creasing trace on the flat sheet. The folding of the box, whether there is surface cracking and the formation of the desired shape should also be included in the inspection record. When a problem is seen, instead of randomly changing a single setting, proceed by comparing material, tooling and machine information.

Short information list for quote and die preparation

• Paperboard manufacturer, product/series name and grammage.
• Measured actual thickness and material sample if possible.
• Grain direction, print, lamination or other surface treatments.
• Exact model of the cutting machine and current counterplate system.
• Scaled drawing, latest revision and expected folding style.

Let's clarify the measurement together

Share your material information along with your drawing. If there is a missing dimension, let's determine this in the technical evaluation; let's not assume the die requirement solely based on grammage.

Explore other cutting die technical guides

Technical preparation and application guides