Edge Tearing in Windowed Paperboard Boxes: Find the Stage Where the Defect Starts
Check edge tearing in windowed paperboard boxes at the window geometry, paperboard properties, cutting, and waste stripping stages.
Fuzzing, crushing, and breakage at the window edge are not the same defect. Before searching for a solution, determining where and during which process the trace formed makes the evaluation more meaningful.
Examine the sample from the front and back surfaces
Mark the problematic edge; record its position on the sheet and grain direction. Compare whether the defect is seen in all ups or only at a specific point. Repeating traces guide the examination; they do not point to the exact cause on their own.
Evaluate the window surroundings together
Check the inner corners, the paperboard between the window and outer cut, and nearby creases. Narrow areas can be stressed while waste is being stripped or panels are being folded. If a corner form or distance change is required, evaluate it over the approved drawing and actual sample.
Complete the paperboard information
Share thickness, grain direction, and surface treatments alongside the grammage. Conduct trials with the actual production paperboard. Do not consider simply increasing pressure as the solution for an edge defect; examine the material, rule condition, and cutting preparation together.
Check the trial in three stages
Re-examine the edges immediately after cutting, when the inner window waste is stripped, and when neighboring folding lines are folded. This makes it easy to distinguish between the trace formed during cutting and the tear growing in the subsequent process.
Prepare for evaluation
• Drawing with separated cutting and creasing lines.
• Actual paperboard and defective sample with markings.
• Front-back surface photos and sheet direction.
• Waste extraction method and current revision.
Share your drawing and defect sample with Özkardeşler; let us clarify the needs for window cutting together.