ÖZKARDEŞLER · TECHNICAL NOTES

Separate Crushing, Folding, and Waste Issues in Corrugated Boxes

Record corrugated box defects separately as crushing, folding, and waste ejection; compare samples using the same reference.

Defects that look similar in corrugated boxes may require different investigations. The first step is to identify where and after which process the issue is observed.

Record the three symptoms separately

Create separate photos and location information for crushed edges, difficult folding, and residual waste. Specify the grain direction. This facilitates re-investigation at the same spot; do not determine the exact cause solely from a photograph.

Include material and setup information

Share flute structure, coating, and batch information. Evaluate cutting, creasing, rubbering, and machine conditions together with the technical team. Do not consider under-cutting in one area as the sole justification for increasing general pressure.

Verify the correction by comparing

Examine the reference and problem samples using the same inspection method. Recheck edges, folding, and output together after the revision. Do not interpret visual correction as fulfilling necessary strength requirements.

Let us clarify your needs together

Share your current drawing, material, and sample information with Özkardeşler; let us evaluate the requirements of your application together.